Creep test

Creep test on plastic films according to DIN EN 13206, DIN 55445 T2, for example T = 23 - 80° C, sample width 10 or 20 mm, testing period as agreed, testing weight as agreed.

In short — AI-generated

The creep test determines how a plastic film deforms under a constant tensile load over a defined period. A strip of film is clamped into the testing device, subjected to a specific weight, and exposed to a controlled temperature to measure the resulting elongation over time.

The test results indicate the material's long-term dimensional stability and resistance to permanent deformation under stress. This data helps developers ensure that packaging or agricultural films will not stretch or fail prematurely when subjected to sustained tension during storage or use.

Text is AI-generated; based on test method data curated and verified by Innoform.

Test Method Group: Mechanical properties

Norms:

Required Sample Amount: sample over total width of material, minimum length: 0,5 m