With circular electrode or polymeric blade electrode (Bayer electrode). Documentation in report as direct result (depending on electrode) and surface resistivity. Conditioning as agreed, measurements even under conditions deviating from the standard climate of 23°C/50% r. h. possible in climate chamber.

Test Method Group: Mechanical properties

Norms:
  • DIN EN 62631-3-2 (VDE 0307-3-2) (2016-10) Dielectric and resistive properties of solid insulating materials - Part 3-1: Determination of resistive properties (DC methods) - Volume resistance and volume resistivity - General method
  • TRGS 727 (2016-07) Technical rule for hazardous substances - avoidance of ignition hazards due to static charges (replacement for TRBS 2153)

Required Sample Amount: Film, paper: sample over total width of material, minimum length: 0,2 m, other samples, per single measurement: min Ø 80 mm (circular electrode) or 100 mm x 30 mm (polymeric blade electrode)

Standard Tests

surface resistance DIN EN 62631-3-2 (hist DIN IEC 60093)

Specific Norm: DIN EN 62631-3-2 (VDE 0307-3-2)

Measurement of the surface resistance after conditioning (96 h) under standard climate (23°C/ 50% r.h.)

surface resistance TRGS 727

Specific Norm: TRGS 727

Measurement of the surface resistance in analogy to DIN EN 62631-3-2 (VDE 0307-3-2 ) with the parallel polymer blade electrode ("Bayer"- electrode) after conditioning (96h) under standard climate (23°C/50% r.h.)

surface resistance TRGS 727-at 23°C/ 30 % r. F.

Specific Norm: TRGS 727

Measurement of the surface resistance in analogy to DIN EN 62631-3-2 (VDE 0307-3-2 ) with the parallel polymer blade electrode ("Bayer"- electrode) after conditioning (96h) under "dry" climate (23°C/30% r.h.)